Applications of BBa_K1321341

As part of our project we carried out an assay to determine the relative binding ability of CBD-sfGFP and sfGFP fusions to bacterial cellulose.

Our first assay was performed to determine the relative strengths of various CBDs’ binding to bacterial cellulose. These were represented by the percentage fluorescence left from CBDs fused to (sfGFP (RFC25)) bound to bacterial cellulose discs, when subjected to various washes. Full protocol can be found ([http://2014.igem.org/Team:Imperial/Protocols here])

In the same assay, results suggested that dCBD, CBDcex, CBDcipA, and C-terminal CBDclos (all fused to sfGFP) had greater ability to bind bacterial cellulose than N-terminal CBDclos. Three washes with dH2O, PBS and 5% BSA were carried out to monitor binding strength. It was determined that the fusion with N-terminal CBDclos was, on average, our fourth strongest CBD, in comparison other CBDs tested.


Figure 1 - CBD binding strength after three dH2O washes.
Figure 2 - CBD binding strength after three 70%Ethanol washes
Figure 3 - CBD binding strength after three PBS washes
Figure 4 - CBD binding strength after three BSA washes